Pure Titanium Plate / Titanium Alloy Sheet Specifications:
Material Grade: Gr1, Gr2, Gr3, Gr4, Gr5, Gr7, Gr6, Gr9, Gr11, Gr12, Gr16, Gr17, Gr25, TA0,TA1,TA2,TA5,TA6,TA7,TA9,TA10,TB2,TC1,TC2,TC3,TC4
Standard ASTM B265, ASME SB265, DIN17851, TiA16Zr5Mo1.5, JIS4100-2007, GB3461-2007
Size:
Cold rolled: Thick 0.02mm ~ 5mm * Wide 1500mm max * Long 2500mm max
Hot rolled: Thick 5mm ~ 100mm * Wide 3000mm max * Long 6000mm max
1. Based on High intensity, titanium products tensile strength can be up to 180Kg/mm².
2. Titanium and titanium alloy in aviation industry, is called “space metal”; In addition, in the shipbuilding industry, chemical industry, manufacturing machinery parts, telecommunications equipment, hard alloy, etc. have increasingly extensive application
3. In addition, because of the titanium alloy with the human body has very good compatibility, so the titanium alloy can also be artificial bone.
6AL-4V titanium Gr5 also known as Ti6Al4V, Ti-6Al-4V, Ti6-4 or Titanium 6Al-4V Alloy, is the most commonly used alloy. It is significantly stronger than commercially pure titanium while having the same stiffness and thermal properties. AMS 4911 6AL-4V titanium sheet & plate is a great selection of aircraft titanium sheet in a variety of specifications.
● Low Density and High Specification Strength.
● Good resistance to effect of heat.
● Low Modulus of Elasticity.
● Good thermal properties.
Grade | N | C | H | Fe | O | Al | V | Pa | Mo | Ni | Ti |
Gr1 | 0.03 | 0.08 | 0.015 | 0.2 | 0.18 | / | / | / | / | / | Bal |
Gr2 | 0.03 | 0.08 | 0.015 | 0.3 | 0.25 | / | / | / | / | / | Bal |
Gr3 | 0.05 | 0.08 | 0.015 | 0.3 | 0.35 | / | / | / | / | / | Bal |
Gr4 | 0.05 | 0.08 | 0.015 | 0.5 | 0.4 | / | / | / | / | / | Bal |
Gr5 | 0.05 | 0.08 | 0.015 | 0.4 | 0.2 | 5.5-6.75 | 3.5-4.5 | / | / | / | Bal |
Gr7 | 0.03 | 0.08 | 0.015 | 0.3 | 0.25 | / | / | 0.12-0.25 | / | / | Bal |
Gr9 | 0.03 | 0.08 | 0.015 | 0.25 | 0.15 | 2.5-3.5 | 2.0-3.0 | / | / | / | Bal |
Gr12 | 0.03 | 0.08 | 0.015 | 0.3 | 0.25 | / | / | / | 0.2-0.4 | 0.6-0.9 | Bal |
Grade | Elongation(%) | Tensile Strength (Min) | Yield Strength (Min) | ||
ksi | Mpa | ksi | Mpa | ||
Gr1 | 24 | 35 | 240 | 20 | 138 |
Gr2 | 20 | 50 | 345 | 40 | 275 |
Gr3 | 18 | 65 | 450 | 55 | 380 |
Gr4 | 15 | 80 | 550 | 70 | 483 |
Gr5 | 10 | 130 | 895 | 120 | 828 |
Gr7 | 20 | 50 | 345 | 40 | 275 |
Gr9 | 15 | 90 | 620 | 70 | 438 |
Gr12 | 18 | 70 | 438 | 50 | 345 |