We insist on offering good quality generation with very good business enterprise concept, honest income as well as best and fast assistance. it will bring you not only the premium quality product or service and huge profit, but probably the most significant is usually to occupy the endless market for Tungsten Carbide Tool, Tungsten Pipe, Titanium Molybdenum Alloy, Winning customers' trust is the gold key to our success! If you are interested in our products, please feel free to visit our web site or contact us.
Short Lead Time for Nimonic Material - CMC CuMoCu Heat Sink – Fotma Detail:

CMC CuMoCu Material Application

Low Expansion Layers and Thermal Paths for Heat Sinks, Lead Frames, Multi-layer Printed Circuit Boards (PCBs), etc.

Heat sink material on aircraft, heat sink material on radar.

CMC CuMoCu Heat Sink (2)

CMC Heat Sink Advantages

1. CMC composite adopts a new process, multilayer copper-molybdenum-copper, the bonding between copper and molybdenum is tight, there is no gap, and there will be no interface oxidation during subsequent hot rolling and heating, so that the bonding strength between molybdenum and copper is excellent, So that the finished material has the lowest thermal expansion coefficient and the best thermal conductivity;

2. The molybdenum-copper ratio of CMC is very good, and the deviation of each layer is controlled within 10%; SCMC material is a multi-layer composite material. The structural composition of the material from top to bottom is: copper sheet – molybdenum sheet – copper sheet – molybdenum sheet… copper sheet, it can be composed of 5 layers, 7 layers or even more layers. Compared with CMC, SCMC will have the lowest thermal expansion coefficient and the highest thermal conductivity.

CMC CuMoCu Heat Sink (1)

Grade of CMC Cu-Mo-Cu Materials

Grade Density g/cm3 Coefficient of thermal Expansion ×10-6  (20℃) Thermal conductivity W/(M·K)
CMC111 9.32 8.8 305(XY)/250(Z)
CMC121 9.54 7.8 260(XY)/210(Z)
CMC131 9.66 6.8 244(XY)/190(Z)
CMC141 9.75 6 220(XY)/180(Z)
CMC13/74/13 9.88 5.6 200(XY)/170(Z)
Material Wt% Molybdenum Content g/cm3 Density Thermal conductivity at 25℃ Coefficient of thermal Expansion at 25℃
S-CMC 5 9.0 362 14.8
10 9.0 335 11.8
13.3 9.1 320 10.9
20 9.2 291 7.4

Product detail pictures:

Short Lead Time for Nimonic Material - CMC CuMoCu Heat Sink  – Fotma detail pictures

Short Lead Time for Nimonic Material - CMC CuMoCu Heat Sink  – Fotma detail pictures

Short Lead Time for Nimonic Material - CMC CuMoCu Heat Sink  – Fotma detail pictures

Short Lead Time for Nimonic Material - CMC CuMoCu Heat Sink  – Fotma detail pictures


Related Product Guide:

We now have a skilled, performance team to supply good quality services for our consumer. We often follow the tenet of customer-oriented, details-focused for Short Lead Time for Nimonic Material - CMC CuMoCu Heat Sink – Fotma , The product will supply to all over the world, such as: Colombia, Venezuela, Denmark, Our organization. Situated inside the national civilized cities, the visitors is very easy, unique geographical and economic situations. We pursue a "people-oriented, meticulous manufacturing, brainstorm, construct brilliant" organization. hilosophy. Strict top quality management, fantastic service, reasonable cost in Myanmar is our stand on the premise of competition. If vital, welcome to make contact with us by our web page or telephone consultation, we are going to be pleased to serve you.
  • Good quality, reasonable prices, rich variety and perfect after-sales service, it's nice!
    5 Stars By Lisa from UK - 2017.03.28 16:34
    It is a very good, very rare business partners, looking forward to the next more perfect cooperation!
    5 Stars By Diego from Rwanda - 2017.06.19 13:51
    Write your message here and send it to us